Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.20 mm
0.0060 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0064 cm/cm

@Thickness 3.20 mm
0.0064 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
2.9 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.9 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength at Break 40.2 MPa
5830 psi
5 mm/min; ASTM D638
Tensile Strength, Yield 41.2 MPa
5970 psi
5 mm/min; ASTM D638
Elongation at Break 17 %
17 %
5 mm/min; ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
5 mm/min; ASTM D638
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.26 GPa
327 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.588 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
1.10 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
0.686 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
1.29 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
1.18 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
1.27 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.39 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C

@Thickness 6.40 mm
241 °F

@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C

@Thickness 6.40 mm
219 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 118 °C
244 °F
B/50; ISO R306
119 °C
246 °F
B/120; ISO R306
Optical Properties Metric English Comments
Yellow Index 31.2 %

@Thickness 31.2 mm
31.2 %

@Thickness 1.23 in
ASTM D1925
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved