Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 7200 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1378 PRE-ELEC PP 1378 is a conductive thermoplastic compound based on glass-fiber reinforced polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electri.. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Melt Flow | 2.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond. I; ASTM D1238 |
Polimeri Europa SINKRAL B532 ABS, Very High Impact
(discontinued **) Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 420 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 788 °F |
ASTM D1238 |
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
(discontinued **) AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 230 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating Borcoat HE3450 is a black, high-density polyethylene (HDPE) produced with the advanced Borstar technology, providing the material with especially well melt strength and extrudability. Also its mech.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
Resin; ISO 1133 |
DuPont Performance Polymers Crastin® CE2056 NC010 PBT Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3300 Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Micropol Isoplas P602 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg |
2.0 g/10 min @Load 11.0 lb |
ASTM D1238/P |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |