Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0064 cm/cm | 0.0064 in/in | SABIC Method |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Linear Mold Shrinkage, Transverse | 0.0064 cm/cm | 0.0064 in/in | ISO 294-4, 2577 |
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1 |
|||
Linear Mold Shrinkage, Transverse | 0.0064 cm/cm @Thickness 3.20 mm |
0.0064 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0064 cm/cm @Thickness 3.20 mm |
0.0064 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0064 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0064 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This .. |