Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.20 GPa | 319 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Ineos ABS Lustran® 723-1, Extrusion Grade
(discontinued **) Extrusion grade for refrigerator inliner.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Ineos ABS Lustran® LGM Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1 |
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1 |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM-D790 |
Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant Flame retardant PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | |
Covestro Makrolon® KU 1-1242/1 Polycarbonate, High Impact High viscosity, impact modified grade with good toughness at low temperatures (dark colors only).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3959 nat PA610 Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Tensile Modulus | 2.20 - 3.50 GPa | 319 - 508 ksi | ASTM D638 |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-2 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 6015 Polycarbonate + PBT Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical .. |
|||
Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |