Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 2.9 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 2.9 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.9 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Melt Flow 2.9 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.9 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Melt Flow 2.9 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film
Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist..
Melt Flow 2.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3500
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 2.9 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.9 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Procedure A; ASTM D1238
Diamond Polymers ASA TW-18B1
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET  (Unverified Data**)
Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size..