Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.9 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.9 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.9 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.9 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.9 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.9 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 2.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3500 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.9 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.9 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ASA TW-18B1 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |