Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.588 J/cm @Temperature -20.0 °C |
1.10 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene Moplen EP300C is the polypropylene blockpolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300C is a block copolymer particularly suitable for sheet and t.. |
|||
Izod Impact, Notched | 0.588 J/cm @Temperature -20.0 °C |
1.10 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP300H Injection Molding Grade Polypropylene Moplen EP300H is a heterophasic copolymer, suitable for injection moulding as well as for thermoforming applications. Moplen EP300H is a excellent low temperature impact behavior combined with a goo.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.10 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.50 mm, Temperature -30.0 °C |
1.10 ft-lb/in @Thickness 0.256 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.10 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.10 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.10 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.10 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.588 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.10 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.35 mm |
1.10 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.35 mm |
1.10 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.588 J/cm @Temperature 0.000 °C |
1.10 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P642J Polypropylene Injection Molding Key Characteristics:Good flowabilityExcellent stiffnessHigh impact strengthMechanical property balanceContains UV stabilizer and anti-static agentRecommended Applications:Industrial and household pr.. |
|||
Izod Impact, Notched | 0.588 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Izod Impact, Notched | 0.588 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger.. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.10 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow 6D20 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr.. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow R131-02A Polypropylene Random Copolymer Resin DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature 23.0 °C |
1.10 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow R132-02A Polypropylene Random Copolymer Resin DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
1.10 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-7107 Rigid PVC, Molding Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it .. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.40 mm |
1.10 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG-1115 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 6.40 mm |
1.10 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.20 mm |
1.10 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1130 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.20 mm |
1.10 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1130 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.587 J/cm @Temperature -18.0 °C |
1.10 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6620A Impact Copolymer Polypropylene High Impact Copolymer for Injection Molding Formolene® 6620A is a copolymer of polypropylene designed and formulated for injection molding applications including pails, crates and furniture. It con.. |
|||
Izod Impact, Notched | 0.588 J/cm @Thickness 3.20 mm |
1.10 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |