Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Samsung, Cheil Industries Product List

Category
Polycarbonate/PET Polyester Blend PBT + ASA Blend, Glass Fiber Reinforced PBT + PET Blend, Glass Filled
PBT + PET, Mineral Filled Polycarbonate, Impact Modified Polycarbonate, 10% Glass Filled
Polycarbonate/ABS Alloy, Unreinforced Polyphenylene Ether, 20% Glass Filled Polycarbonate, Unreinforced, Flame Retardant
Polycarbonate, Molded ABS/Polyester Alloy + GF Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled Polyphenylene Ether, 30% Glass Filled Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Polyphthalamide (PPA), 10% Glass Fiber Reinforced Polycarbonate, 20% Glass Filled Polycarbonate/ABS Alloy, Glass Fiber Filled
Polycarbonate, 30% Glass Filled Polycarbonate, 40% Glass Filled Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler Acrylonitrile Butadiene Styrene (ABS), Molded
ABS/Polyester Alloy Acrylonitrile Butadiene Styrene (ABS), Extruded Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Acrylonitrile Butadiene Styrene (ABS), Plating Grade Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Expanded Polystyrene (EPS) Acrylic, Impact Modified, Molded Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded Polycyclohexylenedimethylene Terephthalate (PCT), 40% Glass Reinforced
Trade Name
Infino® Starex® TRANEX®
Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose PBT + PET, Mineral Filled Infino®
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact Polycarbonate, Impact Modified Infino®
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Polyphenylene Ether, 20% Glass Filled Infino®
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Polycarbonate/ABS Alloy, Unreinforced Infino®
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled Infino®
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Polycarbonate/ABS Alloy, Unreinforced Infino®
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled Nylon Infino®
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Nylon Infino®
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact Polycarbonate, 10% Glass Filled Infino®
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Polyphthalamide (PPA), 10% Glass Fiber Reinforced Infino®
Samsung Cheil Industries Infino® VB-5300G PBT, Glass Filled FR Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Infino®
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Polycarbonate/ABS Alloy, Unreinforced Infino®
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Polycarbonate/ABS Alloy, Unreinforced Infino®
Samsung Cheil Industries Infino® XP-2140 PPS Polyphenylene Sulfide (PPS) Infino®
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler Infino®
Samsung Cheil Industries Infino® XP-2165BM PPS Polyphenylene Sulfide (PPS) Infino®
Samsung Cheil Industries Starex® BF-0670T MABS, Unreinforced Scratch Resistant ABS Polymer Starex®
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant ABS Polymer Starex®
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced ABS/Polyester Alloy Starex®
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled ABS/Polyester Alloy Starex®
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled ABS/Polyester Alloy Starex®
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled Starex®
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled Starex®
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® LH-0300 ABS, Unreinforced Heat Resistant Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded Starex®
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Polystyrene, Impact Modified Starex®
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR Polystyrene, Impact Modified Starex®
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded Starex®
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Molded Starex®
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Acrylonitrile Butadiene Styrene (ABS), Extruded Starex®
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded Starex®
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded Starex®
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced ABS/Polyester Alloy Starex®
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Acrylonitrile Butadiene Styrene (ABS), Extruded Starex®
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded Starex®
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded Starex®
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded Starex®
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant Starex®
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant Starex®
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant Starex®
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Polystyrene, Impact Modified Starex®
Samsung Cheil Industries Starex® VG-4920 ABS, Glass Filled FR Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled Starex®
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled Starex®
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded Starex®
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced Polycarbonate/ABS Alloy, Unreinforced Infino®