Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP640T Injection Molding Grade Polypropylene Moplen EP640T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640T is a block copolymer suitable for injection molding of a.. |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
PolyMirae Moplen EP332C Pipe Extrusion Grade Polypropylene Moplen EP332C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP332C is a block copolymer appreciated by customers in the mar.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.35 mm |
1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.35 mm |
1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
1.29 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.35 mm |
1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.35 mm |
1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature 0.000 °C |
1.29 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm |
1.29 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG-1115 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm |
1.29 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG-1115 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm |
1.29 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X5403 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.686 - 0.883 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 - 1.65 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -20.0 °C |
1.29 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |