Polymer Property : Linear Mold Shrinkage, Transverse = 0.0064 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0064 cm/cm
0.0064 in/in
SABIC Method
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
Linear Mold Shrinkage, Transverse 0.0064 cm/cm
0.0064 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber
PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1
Linear Mold Shrinkage, Transverse 0.0064 cm/cm

@Thickness 3.20 mm
0.0064 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Transverse 0.0064 cm/cm

@Thickness 3.20 mm
0.0064 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Transverse 0.0064 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0064 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..