Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
GRECO ISOPAK 569 ABS Resin Extrusion GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Modulus | 2.26 GPa @Temperature 23.0 °C |
327 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene GA300 Acrylonitrile Butadiene Styrene Applications: injection molding for electrical appliances, toys. |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1006FL PC, Flame Retardant Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | |
Shinil Chemical SHINCON ABS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | |
Shinil Chemical SHINFLAME PC Flame Retardant Polymer Film SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 10 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SC-1220UR PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Trirex® 3015NF Polycarbonate, Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3015NF is a flame retardant grade.Applications: Mobile Phone - battery caseInformation.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0935 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.25 GPa | 327 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA T-115 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.25 GPa | 327 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.25 GPa | 327 ksi | ASTM D-790 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |