Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl GFN1430V PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl GFN1430V PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable water applications and brings potential faster cycle time and lower stress than other 30% glass reinforced Noryl* PPO/PS blends. Noryl* GFN1430V has been certified for potable water applications up to 85C in Europe and North America in limited colours.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D 792
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.060 %
0.060 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
26 g/10 min

@Load 10.0 kg,
Temperature 300 °C
26 g/10 min

@Load 22.0 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
5 mm/min; ISO 527
115 MPa
16700 psi
Type I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 110 MPa
16000 psi
5 mm/min; ISO 527
115 MPa
16700 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 2.2 %
2.2 %
5 mm/min; ISO 527
2.3 %
2.3 %
Type I, 5 mm/min; ASTM D 638
Elongation at Yield 2.2 %
2.2 %
5 mm/min; ISO 527
2.3 %
2.3 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 7.30 GPa
1060 ksi
1 mm/min; ISO 527
8.00 GPa
1160 ksi
5 mm/min; ASTM D 638
Flexural Yield Strength 165 MPa
23900 psi
2 mm/min; ISO 178
169 MPa
24500 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 7.10 GPa
1030 ksi
2 mm/min; ISO 178
7.50 GPa
1090 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.850 J/cm

@Temperature -30.0 °C
1.59 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
0.920 J/cm

@Temperature 23.0 °C
1.72 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 5.20 J/cm

@Temperature 23.0 °C
9.74 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
5.20 J/cm

@Temperature -30.0 °C
9.74 ft-lb/in

@Temperature -22.0 °F
ASTM D 4812
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
30.0 kJ/m²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
30.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 144 °C
291 °F
Rate B/50; ISO 306
149 °C
300 °F
Rate B/50; ASTM D 1525
150 °C
302 °F
Rate B/120; ISO 306
Users viewing this material also viewed the following: