Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 16.0 J | 11.8 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers INDURE™ X190 TPO
(discontinued **) Description: INDURE™ X190 engineered polyolefin material is designed for large, molded-in-color automotive exterior applications that require good scratch and mar characteristics, high stiffness, a.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11 LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Impact Test | 16.0 J @Thickness 3.20 mm |
11.8 ft-lb @Thickness 0.126 in |
Instrumented Total Impact; 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763 |
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Impact Test | 16.0 J | 11.8 ft-lb | tempering temperature 400°C. Austenitizing temperature 1020°C. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |