Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.50 GPa | 1090 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | |
Lehmann & Voss LUVOCOM® 1850/CF/10/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 (Asia Pacific) LNP* Thermocomp* RF00469S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GFT1702-WBK1 33% Glass Fiber Reinforced, Impact Modified and Weatherable Nylon 66 Description: Glass Fiber Reinforced, Impact Modified and Weatherable Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced Developmental productAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | dry; ISO 178 |
DSM EcoPaXX® Q-PG6 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Eurotec® Tecomid® NA40 GR25 NL XA 42 PA 6.6 25% glass fiber reinforced, UL94 V0, red phosphorus Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Beijing Ranger Chem PBT 403 M-G15 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G25 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 7.50 GPa @Temperature 23.0 °C |
1090 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT
(Unverified Data**) Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |