Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 169 MPa | 24500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP HF006EU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF006EU is a compound based on PA 11 resin containing Glass Fiber. Added features include: Easy Molding, UV-Stabilized. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Yield Strength | 169 MPa | 24500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric.. |