Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.850 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.59 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.59 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.59 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.59 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Notched | >= 0.850 J/cm @Temperature 23.0 °C |
>= 1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8300M (EPC30R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
1.59 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.59 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.20 mm, Temperature -18.0 °C |
1.59 ft-lb/in @Thickness 0.126 in, Temperature -0.400 °F |
ASTM-D256 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -29.0 °C |
1.59 ft-lb/in @Temperature -20.2 °F |
ASTM D256 |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -18.0 °C |
1.59 ft-lb/in @Temperature -0.400 °F |
ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This .. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -20.0 °C |
1.59 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 HFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedGood stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.59 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Diamond Polymers NPP25-0604 Impact Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -20.0 °C |
1.59 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -20.0 °C |
1.59 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -20.0 °C |
1.59 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -40.0 °C |
1.59 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature >=0.000 °C |
1.59 ft-lb/in @Temperature >=32.0 °F |
ASTM D256 |
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade .. |