Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26 g/10 min @Load 2.15 kg, Temperature 230 °C |
26 g/10 min @Load 4.74 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® ESD 5400 PRE-ELEC ESD 5400 is a static dissipative thermoplastic compound based on poly-propylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 5400 is developed for t.. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 275 °C |
26 g/10 min @Load 22.0 lb, Temperature 527 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM173R PC UV stabilized PC in special effects colors. Metallic and pearlescent additives. Color may affect performance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 200 °C |
26 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 200 °C |
26 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 300 °C |
26 g/10 min @Load 22.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 280 °C |
26 g/10 min @Load 4.76 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific) A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 300 °C |
26 g/10 min @Load 22.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 230 °C |
26 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat sta.. |
|||
Melt Flow | 26 g/10 min @Load 21.6 kg, Temperature 190 °C |
26 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 38 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® TB 38 HDPE Made for tape applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 245 °C |
26 g/10 min @Load 4.76 lb, Temperature 473 °F |
ISO 1133 |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 300 °C |
26 g/10 min @Load 22.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |