Polymer Property : Flexural Yield Strength = 169 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 169 MPa
24500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific)
LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,..
Flexural Yield Strength 169 MPa
24500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP HF006EU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF006EU is a compound based on PA 11 resin containing Glass Fiber. Added features include: Easy Molding, UV-Stabilized.
Flexural Yield Strength 169 MPa
24500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl GFN1430V PPE+PS
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Flexural Yield Strength 169 MPa
24500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Flexural Yield Strength 169 MPa
24500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Flexural Yield Strength 169 MPa
24500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Flexural Yield Strength 169 MPa
24500 psi
DIN 53455; ASTM D790
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric..