Polymer Property : Impact Test = 16.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 16.0 J
11.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Solvay Engineered Polymers INDURE™ X190 TPO  (discontinued **)
Description: INDURE™ X190 engineered polyolefin material is designed for large, molded-in-color automotive exterior applications that require good scratch and mar characteristics, high stiffness, a..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12
LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC
LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12
LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber.
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East)
Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1430V PPE+PS
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
Impact Test 16.0 J
11.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific)
Glass filled Nylon 12
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Impact Test 16.0 J

@Thickness 3.20 mm
11.8 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber
Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
Impact Test 16.0 J
11.8 ft-lb
tempering temperature 400°C. Austenitizing temperature 1020°C.
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp TX88477 PU
LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.
Impact Test 16.0 J

@Temperature 23.0 °C
11.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..