Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres
PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral
PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral
PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl V01505 PPE+HIPS
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
Phr = 5
Shandong Rike Chemical ACM-1 PVC Impact Modifier ACM Resin
Outline of ACM ResinFor overcoming the shortcomings of plasticizers and CPE, we developed a new type impact modifier ACM which as a copolymer of HDPE and acrylic acid and our ACM not only has the ba..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX5121 PBT (Europe-Africa-Middle East)
VALOX VX5121 is a 15 % glass reinforced PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl GFN1430V PPE+PS
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable..