Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ MX5210-0040 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-40G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-40G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Nilit FRIANYL B63 KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Nilit FRIANYL B63 TF-GV 1530 Nylon 6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.10 GPa @Temperature 23.0 °C |
1030 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B12^ F30 AS Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178-93 |
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178-93 |
Wellman EcoLon® MRGF1878-BK1 Nylon 6, 30% Mineral/Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 275 Polystyrene Alloy, Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)