Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Screen Pack: 60/60 Screw: 3:1 to 3.5:1 compression ratio screw PVC screwInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Viscosity 35000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
1.20e+6 cP

@Shear Rate 67.0 1/s,
Temperature 200 °C
1.20e+6 cP

@Shear Rate 67.0 1/s,
Temperature 392 °F
ASTM D3835
Maximum Moisture Content 0.020
0.020
Deformation 40 %

@Temperature 150 °C
40 %

@Temperature 302 °F
300g; UL 1581
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
10 sec; ASTM D2240
Tensile Strength at Break 24.1 MPa
3500 psi
UL 1581
17.9 MPa

@Temperature 23.0 °C
2600 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 240 %
240 %
UL 1581
240 %

@Temperature 23.0 °C
240 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Electrical Properties Metric English Comments
Dielectric Constant 2.42

@Frequency 50.0 Hz
2.42

@Frequency 50.0 Hz
IEC 60250-1969; IEC 60250
Dielectric Strength 51.0 kV/mm
1300 kV/in
IEC 60243-1
Dissipation Factor 0.0060
0.0060
TangentTest condition: 50 Hz IEC 60250-1969; IEC 60250
Processing Properties Metric English Comments
Zone 1 180 - 190 °C
356 - 374 °F
Zone 2 185 - 200 °C
365 - 392 °F
Zone 3 185 - 210 °C
365 - 410 °F
Zone 4 185 - 210 °C
365 - 410 °F
Die Temperature 195 - 220 °C
383 - 428 °F
Drying Temperature 70.0 - 81.1 °C
158 - 178 °F
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Descriptive Properties Value Comments
Appearance Natural Color
Features Flame Retardant
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Wire & Cable Applications
VW-1 pass
UL 1581