Polymer Property : Viscosity = 35000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 35000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af..
Viscosity 35000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-..
Viscosity 35000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Viscosity 35000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Viscosity 35000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE)
Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat ..
Viscosity 35000 cP

@Temperature -30.0 °C
35000 cP

@Temperature -22.0 °F
MRV
ExxonMobil Mobil Clean 10W-40 Motor Oil
Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes..
Viscosity 35000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
35000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It..
Viscosity 35000 cP

@Temperature -30.0 °C
35000 cP

@Temperature -22.0 °F
MRV
ExxonMobil Mobil Clean 10W-40 Motor Oil
Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes..
Viscosity 35000 cP

@Temperature 25.0 °C
35000 cP

@Temperature 77.0 °F
BASF Pluracol® SG-470 Rigid Polyol
Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent ..
Viscosity 35000 cP

@Temperature 25.0 °C
35000 cP

@Temperature 77.0 °F
BASF Pluracol® SG-450 Rigid Polyol
Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent ..