A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion in combination with good impact strength. Typical applications would include automotive claddings and rocker panels. TPP 518 is paintable and can be provided UV stable.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Melt Index of Compound 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Gardner Impact 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C

@Temperature 20.0 °C
34.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Brittleness Temperature -30.0 °C
-22.0 °F