Polymer Property : Dry Time = 8.00 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Desiccant Dryer
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66)
Information provided by PolyOne
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Desiccant Dryer
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66)
Information provided by PolyOne
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
Dry Time 4.00 - 8.00 hour

@Temperature 120 °C
4.00 - 8.00 hour

@Temperature 248 °F
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Dry Time 4.00 - 8.00 hour

@Temperature 120 °C
4.00 - 8.00 hour

@Temperature 248 °F
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS.
Dry Time 4.00 - 8.00 hour

@Temperature 120 °C
4.00 - 8.00 hour

@Temperature 248 °F
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
Dry Time 4.00 - 8.00 hour

@Temperature 120 °C
4.00 - 8.00 hour

@Temperature 248 °F
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment
PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS.
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Celanese VECTRA B230 LCP, 30% Specialty
Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced.Information provided by Celanese
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Handling
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Handling
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Touch
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Recoat
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Handling
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Recoat
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled
Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C).
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)  (Unverified Data**)
Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili..
Dry Time 4.00 - 8.00 hour

@Temperature 120 °C
4.00 - 8.00 hour

@Temperature 248 °F
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
Dry Time 6.00 - 8.00 hour
6.00 - 8.00 hour
DAM
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo..