Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
23/23°C; ASTM D792
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Polymax® Maxelast® P3880H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.02 g/cc
1.02 g/cc
NuSil CV10-2500 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: High Durometer, Optically ClearCure system: PlatinumInformation provided by NuSil
Specific Gravity 1.02 g/cc
1.02 g/cc
NuSil CV-2500 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: Pourable, Optically ClearCure system: PlatinumInformation provided by NuSil
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Polymax® Maxelast® P1955 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D 792
RTP Company RTP 6003-75A UV Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT - UV Stabilized
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D 792
RTP Company RTP 6003-75A Z Specialty Thermoplastic Elastomer, FDA Compliant Ingredients
Specific Gravity 1.02 g/cc
1.02 g/cc
NuSil CV-2501 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: Longer Work Time, Optically ClearCure system: PlatinumInformation provided by NuSil
Specific Gravity 1.02 - 1.08 g/cc
1.02 - 1.08 g/cc
Uncured
Resin Technology Group UV-403 High Clarity, Structural Polycarbonate and PVC Bonder
UV 403 is a very fast UV curing adhesive developed for bonding a variety of plastics. Bond strengths on polycarbonate and rigid PVC usually exceed the strength of those substrates. Bond lines are cl..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Specific Gravity 1.02 - 1.04 g/cc
1.02 - 1.04 g/cc
Michelman® Michem® Coat 50 AFN Fluorocarbon free, water and grease resistant coating
Description: Fluorocarbon free, water and grease resistant coatingUsage: Michem® Coat 50AFN is an oil and grease resistant coating which also imparts good water resistance. This product is flexo ..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 1.02 g/cc
1.02 g/cc
Teknor Apex Tekbond® TB 2001 Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 372 Ionomer
Information provided by A. Schulman.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D 792
RTP Company ESD C 2800 B-55A Black Thermoplastic Polyolefin Elastomer (TEO), Electrically Conductive - ESD Protection
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D 792
RTP Company RTP 2800 B-75A HF UV Thermoplastic Polyolefin Elastomer (TEO) High Flow - UV Stabilized
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 397 Ionomer
Information provided by A. Schulman.
Specific Gravity 1.02 g/cc

@Temperature 25.0 °C
1.02 g/cc

@Temperature 77.0 °F
Dow Corning MOLYKOTE® PG-54 PLASTISLIP GREASE
Silicone grease with solid lubricantsInformation provided by Dow Corning
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy
Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ..
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® 430 Epoxy
Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding ..
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® 921 Thermally Conductive Epoxy
Material Description: A two component, high Tg, electrically insulating, thermally conductive epoxy designed for thermal management applications found in semiconductor, hybrid microelectronics, PCB,..
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy
Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Specific Gravity 1.02 g/cc
1.02 g/cc
"A" component
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating
QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: ..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 30424 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 30424 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in blow molding and injection molding applications. POLYBATCH® 3042..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D 792
RTP Company RTP 2740 U-70A Unsaturated Styrenic Block Copolymer  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
RTP Company ESD C 2800 Value-added Thermoplastic Polyolefin Elastomer, ESD Protection  (discontinued **)