Polymer Property : Specific Gravity = 1.02 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
23/23°C; ASTM D792
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Polymax® Maxelast® P1860D TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Polymax® Maxelast® P3875 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Polymax® Maxelast® P3890 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
PB1100-60 Polyurethane-based Biomedical Elastomer
Specific Gravity 1.02 g/cc
1.02 g/cc
Resinlab® RC8038 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Specific Gravity 1.02 g/cc
1.02 g/cc
23/23°C; ASTM D792
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.02 g/cc
1.02 g/cc
Silicone Rubber; JIS K6249/ASTM D792
Fujipoly Industries FG-S Fine Connector
Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Specific Gravity 1.02 - 1.04 g/cc
1.02 - 1.04 g/cc
Michelman® Plate Kote™ 980 KOSHER Water based OPV
Description: Water based OPV for paper platesUsage: Plate Koteâ„¢ 980 is a food-contact compliant release coating which has been formulated solely for the unique requirements of paper plate conve..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer
Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product
DescriptionPOLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBAT..
Specific Gravity 1.02 g/cc
1.02 g/cc
Zylog Hipolyene® 3152 MC Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 372 Ionomer
Information provided by A. Schulman.
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer
Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T..
Specific Gravity 1.02 - 1.06 g/cc
1.02 - 1.06 g/cc
ASTM D792
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene
DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman.
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product
DescriptionPOLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBAT..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 30424 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 30424 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in blow molding and injection molding applications. POLYBATCH® 3042..
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy
Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353..
Specific Gravity 1.02 g/cc
1.02 g/cc
Part B
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy
Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing..
Specific Gravity 1.02 g/cc

@Temperature 25.0 °C
1.02 g/cc

@Temperature 77.0 °F
Dow Corning 2-3896 Antifoam Compound
100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning
Specific Gravity 1.02 g/cc
1.02 g/cc
Laminate; ISO 2577
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Buckeye Polymers BP FLEX D5718 TU BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Specific Gravity 1.02 g/cc
1.02 g/cc
Uncatalyzed, QM 262B
ACC QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..
Specific Gravity 1.02 g/cc
1.02 g/cc
hardener
BCC Products BC 8660E Urethane Elastomer
BC8660E is a multi-purpose elastomer that can perform many functions. Special product characteristics are: excellent use for molds for casting of concrete and plaster, resists moisture absorption, d..