Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.007848 GPa

@Temperature 110 °C,
Time 86400 sec
1.138 ksi

@Temperature 230 °F,
Time 24.0 hour
0.017658 GPa

@Temperature 1500 °C,
Time 10800 sec
2.5611 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
49.0 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage 0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
0.98 %

@Temperature 1500 °C,
Time 10800 sec
0.98 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 64 %
64 %
SiO2 31 %
31 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Main Applications Tundish
Material Required for Estimating (kg/?) 2,600
Water Required for Casting(%) 7.1