Polymer Property : Zone 3 = 210 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 185 - 210 °C
365 - 410 °F
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af..
Zone 3 190 - 210 °C
374 - 410 °F
Extruder
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for ..
Zone 3 193 - 210 °C
380 - 410 °F
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene  (Unverified Data**)
ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st..
Zone 3 193 - 210 °C
380 - 410 °F
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to..
Zone 3 193 - 210 °C
380 - 410 °F
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm..
Zone 3 193 - 210 °C
380 - 410 °F
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene
ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont..
Zone 3 193 - 210 °C
380 - 410 °F
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene
ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant ..
Zone 3 190 - 210 °C
374 - 410 °F
Blow Molding
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Zone 3 190 - 210 °C
374 - 410 °F
Blow Molding
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
Zone 3 200 - 210 °C
392 - 410 °F
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Zone 3 200 - 210 °C
392 - 410 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil..
Zone 3 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 3 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by..
Zone 3 193 - 210 °C
379 - 410 °F
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled
Data provided by Clariant Masterbatches
Zone 3 190 - 210 °C
374 - 410 °F
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene
OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA..