Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP7033N Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7033N Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics and improved cycle time.Availability: North America and Asia Pacific Features:Balanced Stiffness/ToughnessFast Molding CycleMedium FlowHigh Impact ResistanceHigh StiffnessNucleatedUses: ApplianceAutomotive ApplicationsChild Safety SeatsConsumer Applications Industrial ApplicationsRigid PackagingProcessing Method: Injection MoldingAutomotive Specifications: Hyundai MS213-26 Type 1 (Approval specific to USA sourced material)Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.8 MPa
3740 psi
ISO 527-2/50
25.9 MPa
3760 psi
2 in/min; ASTM D638
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
5.2 %
5.2 %
2 in/min; ASTM D638
Tensile Modulus 1.32 GPa
192 ksi
ISO 527-2/1
Flexural Modulus 1.25 GPa
182 ksi
0.079 in/min; ISO 178
1.36 GPa
197 ksi
1% secant, 0.05 in/min.; ASTM D790
1.54 GPa
224 ksi
1% secant, 0.5 in/min; ASTM D790B
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 3.99 kJ/m²

@Temperature -40.0 °C
1.90 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
4.83 kJ/m²

@Temperature -17.8 °C
2.30 ft-lb/in²

@Temperature 0.000 °F
ISO 180/1A
12.8 kJ/m²

@Temperature 22.8 °C
6.10 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Charpy Impact, Notched 4.62 J/cm²

@Temperature -30.0 °C
22.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
5.25 J/cm²

@Temperature -20.0 °C
25.0 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
7.35 J/cm²

@Temperature 0.000 °C
35.0 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
13.0 J/cm²

@Temperature 22.8 °C
61.9 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Gardner Impact 22.4 J

@Thickness 3.17 mm,
Temperature -30.0 °C
16.5 ft-lb

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.7 °C
197 °F
ISO 75-2/A
107 °C
225 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ISO 75-2/Bf
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved