Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.62 J/cm² @Temperature -30.0 °C |
22.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |