Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S USZ200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ B700 X2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eA |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 22.8 °C |
61.9 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Charpy Impact, Notched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S ESL128 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |