Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ CA278A Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA278A is a thermoplastic polyolefin elastomer that is used for automotive interior partsFeatures: Good StiffnessHigh FlowGood MoldabilityGood Impact ResistanceLow Temper.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ASTM D648 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil Exxtral™ LNV 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high gloss, low warpage, and low discoloration in contact with hot water/steam in large electrical appliance such as washing mach.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil PP1013H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil PP1014H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil PP1063L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/A |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | ISO 75-2/Bf |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334C10L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | |
Aclo Accutech Polypropylene Copolymer CP0436T10L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifax™ HSBMF248 Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMF248 high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of flow, rigidity, low t.. |