Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | Injection Molding; ASTM D256 |
Network Polymers NPS 90-0304 F Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total Finathene® CD 522 HDPE corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
0.125"; ASTM D256 |
LTL Color Compounds ColorRxâ„¢ ABS-0500RX Biocompatible ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
0.125"; ASTM D256 |
LTL Color Compounds ColorRxâ„¢ ABS-0502ARX Biocompatible, Antimicrobial ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS FR V2 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | 1/8 in sample; ASTM D256 |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® PC-50/TF/13/SI/2 BK3585 Polycarbonate |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | Crosswise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Izod Impact, Notched | 2.14 - 2.67 J/cm | 4.00 - 5.00 ft-lb/in | |
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in .. |
|||
Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPU 0445 A Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc. |