Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Nilit Nilitop BT FR C3 Unfilled, Flame Retardant PBT Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive.Key characteristics: Go.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 180 |
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A28 PA66, Injection Molding Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR560B1 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B1 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 3.99 kJ/m² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL FA 50 PA 6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifax™ HSBMCB1158LS Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impa.. |
|||
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East) 15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |