Polymer Property : Izod Impact, Notched = 2.14 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.14 J/cm

@Temperature 23.0 °C
4.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
1/8 in specimen; ASTM D256
Network Polymers Nylon 6040
Description: Natural NylonInformation provided by Network Polymers Inc.
Izod Impact, Notched 2.14 J/cm

@Temperature 22.8 °C
4.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow
Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM)
Information provided by Ravago.
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 300 TFE 15 SE Polycarbonate (PC), Unreinforced - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-2
RTP 300 TFE 15 SE is an internally lubricated polycarbonate which exhibits low wear characteristics while maintaining the toughness and self-extinguishing behavior of the base resin.
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256-93a
Multibase Multi-Pro® 5002 X White 50% Filler Content Polypropylene
Multi-Pro 5002 X White is an extrusion grade filled polypropylene that has good stiffness as well as excellent impact properties. It can be made in any color.Data provided by Multibase.
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 2299 X 68910 A  Polyetheretherketone (PEEK) Long Glass Fiber 40%  (discontin
Long Glass Fiber 40%Comments:Long Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company..
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256A
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin  (discontinued **)
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Albis Plastics ASA 02A 811 Unreinforced  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..
Izod Impact, Notched 2.14 - 3.20 J/cm
4.00 - 6.00 ft-lb/in
ASTM D256
Premix Premi-Glas® 1201-10 Polyester SMC  (discontinued **)
Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
Izod Impact, Notched 2.14 - 3.20 J/cm
4.00 - 6.00 ft-lb/in
ASTM D256
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc.
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 2610 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 2.14 J/cm

@Temperature 23.0 °C
4.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene
Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat..
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company PermaStat® 600 Nat/Clear Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static - Transparent Grade
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2300 A FR Rigid Thermoplastic Polyurethane (RTPU), Flame Retardant
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 2599 X 61232 A FR Polycarbonate/ABS Alloy (PC/ABS), PTFE Lubricated - Flame Retardant - Bromine/Chlorine Free - UL94 V-0
Izod Impact, Notched 2.14 J/cm

@Thickness 3.20 mm
4.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company ESD 3283 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Electrically Conductive
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1205 T-70A Ether-based Thermoplastic Polyurethane Elastomer, Glass Fiber Reinforced
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS VP-11 SHF
Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Celanese Celstran® PP-GF30-02 PP, 30% Glass Reinforced
30% long strand glass fiber reinforced polypropylene30% long strand glass fiber reinforced, chemically coupled polypropyleneInformation provided by Celanese
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Chem Polymer Chemlon 267 Nylon 6, Impact Modified
An extrusion grade copolymer nylon 6, providing good melt strength, impact, elongation, and flexibility. This grade provides excellent properties in most convoluted tubing or wire coating applicati..
Izod Impact, Notched 2.14 - 3.20 J/cm
4.00 - 6.00 ft-lb/in
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext..
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 3199 X 120865 D Perfluoroalkoxy (PFA), Carbon Fiber
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Izod Impact, Notched 2.14 - 3.20 J/cm
4.00 - 6.00 ft-lb/in
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound
BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes..