Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 22.4 J @Thickness 3.17 mm, Temperature -30.0 °C |
16.5 ft-lb @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D5420 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |