Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.25 GPa | 182 ksi | ASTM D790 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1452S (H39S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 7445L (EPC57MA) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Polimeri Europa Eraclene® MQ 70 U High Density Polyethylene - Injection Molding Eraclene MQ 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a mediu.. |
|||
Flexural Modulus | 1.25 GPa @Thickness 3.17 mm |
181 ksi @Thickness 0.125 in |
injection molded specimen, 2 mm/min; ISO 178 |
Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued .. |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4052V (52418) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Flexural Modulus | 1.25 - 3.05 GPa @Temperature 60.0 - 120 °C |
181 - 442 ksi @Temperature 140 - 248 °F |
Average value: 1.97 GPa Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Iran Petrochemical (PCC) 6040UA High Density Polyethylene HD-6040UA is an ultra-violet light stabilized high density polyethylene injection grade with a narrow molecular weight distribution, specially developed for injection molding of heavy duty parts for.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR30MC2 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection molding. Lumicene® MR30MC2 differs from the other random copolymers by its molding reproduci.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet TOTAL Petrochemicals Polypropylene 4252 is a 1.5 melt flow rate impact copolymer designed for improved toughness and high melt strength. This resin offers outstanding processability in combination .. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Total PPC 5946WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total PPH 7089 Polypropylene Homopolymer, Fiber Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Borealis RD360MO Polypropylene Random Copolymer, Transparent RD360MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleating and ant.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 503 Polypropylene Impact Copolymer Made for injection molding applications. Basic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 527-2 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Total PPC 5945WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5945WZ is a nucleated impact copolymer with a Melt Flow index of 80 g/10 min.TOTAL Polypropylene 5945WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Xsene® XS10 H HDPE, pipe, injection molding FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound.. |
|||
Flexural Modulus | 1.25 GPa | 182 ksi | 0.079 in/min; ISO 178 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | SAE J949 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SG 50 Polypropylene Impact Copolymer Description: CAPILENE® SG 50 is a low melt flow rate impact copolymer suitable for injection molding applications. It exhibits good stiffness combined with high impact strength.Applications: CAP.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SL 50 Polypropylene Impact Copolymer Description: CAPILENE® SL 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade combines good stiffness and impact properties.Applications: CAPILENE® SL .. |
|||
Flexural Modulus | >= 1.25 GPa | >= 181 ksi | ISO 178 |
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Flexural Modulus | 1.25 GPa | 181 ksi | ISO 178 |
Total Finathene® SI 508 HDPE blow molding
(discontinued **) Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weig.. |