Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.9 MPa | 3760 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP H6 GF25 NHFR grey Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-3701 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CM100LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding Medium impact, nucleated, antistat, injection molding. Applications: Household articles, pails, consumer products.Information provided by Phillips 66. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer COPYLENE® CM005 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes..Applications: Extrusion, sheet, film.Infor.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CM020N Polypropylene Impact Copolymer COPYLENE® CM020N is a nucleated, medium impact copolymer with an excellent balance of stiffness and impact performance for extrusion and injection processes.Applications: Extrusion and Injection Mo.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | at 2 in/min; ASTM D638 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2 in/min; ASTM D638 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
Dow C700-35 Polypropylene Impact Copolymer Resin OverviewHigh stiffnessGood mold fillabilityComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35 Polypropylene Resin is intended for use in injection molding processes where medium .. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | molded and tested in accordance with ASTM D 4101; ASTM D638 |
Dow C700-35 Polypropylene Resin DOW C700-35 is intended for use in injection molding processes where medium impact strength is required.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in J.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | ASTM D638 |
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | |
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | ASTM D-638 |
Axiall 36431 Coax & Telecom Flexible PVC 80°C rated, semi-rigid insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Tensile Strength, Yield | 25.9 MPa | 3750 psi | ASTM D638 |
Multibase Multi-Flam™ 0106 PP Polypropylene Features:Flame RetardantHalogenated Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 25.9 MPa | 3760 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® PD2000 Polypropylene DescriptionPolyaxis PD 2000 is a polypropylene specifically designed from rotational molding.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and E.. |