Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.54 GPa | 223 ksi | Tangent, Injection Molded Sample, 0.05 in/min test speed; ASTM D790 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Flexural Modulus | 1.54 GPa | 223 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11 LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System |
|||
Flexural Modulus | 1.54 GPa | 223 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Flexural Modulus | 1.54 GPa | 224 ksi | 1% secant, 0.5 in/min; ASTM D790B |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Flexural Modulus | 1.54 GPa @Temperature 65.0 °C |
223 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
Flexural Modulus | 1.54 GPa | 223 ksi | ASTM D790 |
Amco PRIMATOP HDPE RP 004 Granular High Density Polyethylene HDPE RP 004 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 1.54 GPa | 223 ksi | ASTM D790 |
Braskem CP 145 Injection Molding Polypropylene Applications: Household; thin-walled parts; easy mould filling. Information provided by Braskem |