EMS-Grivory Grivory® ELX 50 HNZ TPA

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® ELX 50 HNZ TPA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the following important properties: Very high melt strengthVery high flexibilityExcellent toughness at low temperaturesProcessable on conventional as well as on 3 D-machinesSuitable for sequential blow molding technology Grilon ELX 50 H NZ is used typically as flexible part in the sequential blow molding technology in combination with a rigid PA6 grade such as Grilon EB 50 H or Grilon R 50 H NZ or Grilon EBV-15H. Application examples are air ducts for turbo-chargers and engine air ducts.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption 6.5 %
6.5 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
conditioned, 15s; ISO 868
50
50
dry, 15s; ISO 868
Tensile Stress 12.0 MPa

@Strain 50.0 %
1740 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.150 GPa
21.8 ksi
conditioned; ISO 527-1/-2
0.220 GPa
31.9 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
Melting Point 210 °C
410 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 35.0 °C
95.0 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
conditioned; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 29.0 kV/mm
737 kV/in
dry; IEC 60243-1
30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 575 V
575 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Extrusion - blow molding
Other Extrusion
Special Characteristics High impact or impact modified
Improved heat resistance