Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 210 - 220 °C | 410 - 428 °F | ISO 11357-1 |
Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Appl.. |
|||
Melting Point | 210 °C | 410 °F | |
Radici Radilon® S 40EP3215 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Melting Point | 210 °C | 410 °F | ASTM D789 |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 210 °C | 410 °F | DIN 53736 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
Melting Point | >= 210 °C | >= 410 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® ECO PA GF30 909040 Nylon 6, 30% Glass Fiber PA 6 (mainly), 30% glass fibers, injection molding, contains at least 80% pre-consumer recycled material, properties may change considerably from lot to lotInformation provided by LANXESS. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | ASTM D789 |
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 210 - 220 °C | 410 - 428 °F | Huntsman/TMA |
Huntsman IROGRAN® A 95 K 4977 TPU-High Temperature Performance Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov.. |
|||
Melting Point | 210 °C | 410 °F | ASTM D2117 |
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5450 is an extrusion grade.Information provided by Samyang. |
|||
Melting Point | 210 °C | 410 °F | by DSC, 10°C per 210 minutes |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Melting Point | 210 °C | 410 °F | By DSC |
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Melting Point | 210 - 212 °C | 410 - 414 °F | |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFLEX P D63.1 Polyester-Elastomer, Shore D63 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 210 °C | 410 °F | ASTM D789 |
Chem Polymer Chemlon 253 H Nylon 6, Impact Modified A medium viscosity impact modified, heat stabilized nylon 6 exhibiting improved toughness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 413 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 °C | 410 °F | ASTM D3418 |
Ashley Polymers Ashlene® 734LD Nylon 6 A plasticized, highly flexible Nylon 6 with high impact resistance.Data provided by the manufacturer |
|||
Melting Point | 210 °C | 410 °F | ASTM D3418 |
Ashley Polymers Ashlene® 737 Nylon 6 A modified nylon for applications requiring exceptional flexibility for extrusion.Data provided by the manufacturer |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Comtuf® 463 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 210 °C | 410 °F | |
Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melting Point | 210 °C | 410 °F | by DSC, 10°C per 210 minutes |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |