Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | >= 0.150 GPa | >= 21.8 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | >= 0.150 GPa | >= 21.8 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.150 GPa | 21.8 ksi | ASTM D638 |
Solvay Specialty Polymers solvene® T 2808 Electroactive Polymer (EAP) Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/.. |
|||
Tensile Modulus | 0.150 GPa | 21.8 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Tensile Modulus | 0.150 GPa @Temperature 120 °C |
21.8 ksi @Temperature 248 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |
|||
Tensile Modulus | 0.150 GPa @Temperature 120 °C |
21.8 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Tensile Modulus | 0.150 GPa | 21.8 ksi | 1 mm/min |
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |