Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | DTUL Unannealed; ASTM D648 |
Network Polymers NPP 11-0535 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 - 118 °C | 122 - 245 °F | Average value: 95.9 °C Grade Count:65 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-2 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
DSM Somos® 9110 Epoxy Photopolymer DescriptionDSM Somos® 9110 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | Unannealed (0.250 in); ASTM D648 |
Entec Hypel® PELLD5/.935 LLDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Diamond Polymers NPP11-0635 Medium Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | <= 50.0 °C | <= 122 °F | |
C.O.I.M. EXTER S® S 902 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 902: Flexible resin .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-2 |
CENTROPLAST BC Organic Thermoplastic CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting accordin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |