Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.0 MPa @Strain 100 %, Temperature 135 °C |
2320 psi @Strain 100 %, Temperature 275 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PB420 TPC-ET Blow Molding Grade |
|||
Tensile Stress | 16.0 MPa @Strain 50.0 % |
2320 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Tensile Stress | 16.0 MPa @Strain 50.0 % |
2320 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Tensile Stress | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.0 MPa @Strain 10.5 %, Time 3.60e+6 sec |
2320 psi @Strain 10.5 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 16.0 MPa @Strain 7.73 %, Time 36000 sec |
2320 psi @Strain 7.73 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 16.0 MPa @Strain 12.1 %, Time 3.60e+7 sec |
2320 psi @Strain 12.1 %, Time 10000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 16.0 MPa @Time 3600 sec, Strain 6.63 % |
2320 psi @Time 1.00 hour, Strain 6.63 % |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 16.0 MPa @Strain 9.05 %, Time 360000 sec |
2320 psi @Strain 9.05 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 16.0 MPa @Strain 50.0 % |
2320 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.0 MPa @Strain 0.450 %, Temperature 150 °C |
2320 psi @Strain 0.450 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 16.0 MPa @Strain 21.29 %, Temperature 90.0 °C |
2320 psi @Strain 21.29 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Tensile Stress | 16.0 MPa @Strain 10.0 % |
2320 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
2320 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Tensile Stress | 16.0 MPa @Strain 50.0 % |
2320 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 16.0 MPa @Strain 300 % |
>= 2320 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 16.0 MPa @Strain 5.00 % |
2320 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Tensile Stress | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Tensile Stress | 16.0 MPa @Strain 2.30 %, Temperature 40.0 °C |
2320 psi @Strain 2.30 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |