Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.220 GPa | 31.9 ksi | TD |
Kuraray HYBRAR® CF2 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.220 GPa | 31.9 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Tensile Modulus | 0.220 GPa @Temperature 120 °C |
31.9 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8253 PA6 (Conditioned) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |