Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 16.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 16.0 MPa

@Strain 100 %,
Temperature 135 °C
2320 psi

@Strain 100 %,
Temperature 275 °F
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Tensile Stress 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PB420 TPC-ET
Blow Molding Grade
Tensile Stress 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® ELX 40 HNZ TPA
Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow..
Tensile Stress 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
dry; ISO 527-1/-2
EMS-Grivory Grivory® ELX 50 HNZ TPA
Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi..
Tensile Stress 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 16.0 MPa

@Strain 10.5 %,
Time 3.60e+6 sec
2320 psi

@Strain 10.5 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 16.0 MPa

@Strain 7.73 %,
Time 36000 sec
2320 psi

@Strain 7.73 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 16.0 MPa

@Strain 12.1 %,
Time 3.60e+7 sec
2320 psi

@Strain 12.1 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 16.0 MPa

@Time 3600 sec,
Strain 6.63 %
2320 psi

@Time 1.00 hour,
Strain 6.63 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 16.0 MPa

@Strain 9.05 %,
Time 360000 sec
2320 psi

@Strain 9.05 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 16.0 MPa

@Strain 0.450 %,
Temperature 150 °C
2320 psi

@Strain 0.450 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 16.0 MPa

@Strain 21.29 %,
Temperature 90.0 °C
2320 psi

@Strain 21.29 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..
Tensile Stress 16.0 MPa

@Strain 10.0 %
2320 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 16.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
2320 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**)
Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon ..
Tensile Stress 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 16.0 MPa

@Strain 300 %
>= 2320 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 16.0 MPa

@Strain 5.00 %
2320 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® CM600-V TPC-ES FR
Extrusion, Flame Retardant (Halogen free)
Tensile Stress 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® CM600-V TPC-ES FR
Extrusion, Flame Retardant (Halogen free)
Tensile Stress 16.0 MPa

@Strain 2.30 %,
Temperature 40.0 °C
2320 psi

@Strain 2.30 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved