| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.31 g/cc | 1.31 g/cc | DAM; ASTM D792 |
| Density | 1.30 g/cc | 0.0470 lb/in³ | DAM; ISO 1183 |
| Filler Content | 15 % | 15 % | DAM |
| Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 1.60 mm |
0.0040 in/in @Thickness 0.0630 in |
Flow; DAM |
| 0.0045 cm/cm @Thickness 3.20 mm |
0.0045 in/in @Thickness 0.126 in |
Flow; DAM | |
| 0.010 cm/cm @Thickness 1.60 mm |
0.010 in/in @Thickness 0.0630 in |
Transverse; DAM | |
| 0.011 cm/cm @Thickness 3.20 mm |
0.011 in/in @Thickness 0.126 in |
Transverse; DAM | |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Thickness 2.00 mm |
0.0060 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 110 MPa @Temperature 23.0 °C |
16000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Strength | 123 MPa @Temperature 23.0 °C |
17800 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
| Elongation at Break | 2.0 % @Temperature 23.0 °C |
2.0 % @Temperature 73.4 °F |
DAM; ASTM D638 |
| 2.0 % @Temperature 23.0 °C |
2.0 % @Temperature 73.4 °F |
DAM; ISO 527 | |
| Tensile Modulus | 6.50 GPa @Temperature 23.0 °C |
943 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Strength | 162 MPa @Temperature 23.0 °C |
23500 psi @Temperature 73.4 °F |
DAM; ASTM D790 |
| Flexural Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| 6.21 GPa @Temperature 23.0 °C |
901 ksi @Temperature 73.4 °F |
DAM; ASTM D790 | |
| Izod Impact, Notched | 0.530 J/cm @Temperature 23.0 °C |
0.993 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
| 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
| 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
| 300 °C | 572 °F | DAM; ASTM D3418 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 276 °C | 529 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | DAM; ASTM D648 |
| 250 °C | 482 °F | DAM; ISO 75-1/-2 | |
| UL RTI, Electrical | 150 °C @Thickness 3.00 mm |
302 °F @Thickness 0.118 in |
DAM; UL 746B |
| 150 °C @Thickness 0.750 mm |
302 °F @Thickness 0.0295 in |
DAM; UL 746B | |
| 150 °C @Thickness 1.50 mm |
302 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
DAM; UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 150 °C @Thickness 3.00 mm |
302 °F @Thickness 0.118 in |
DAM; UL 746B | |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
DAM; UL94 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; UL94 | |
| HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
DAM; UL94 | |
| Oxygen Index | 23 % | 23 % | DAM; ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
| Surface Resistance | 1.00e+16 ohm @Temperature 23.0 °C |
1.00e+16 ohm @Temperature 73.4 °F |
DAM; IEC 60093 |
| Dielectric Constant | 3.7 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.7 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; IEC 60250 |
| 4.0 @Frequency 1000 Hz, Temperature 23.0 °C |
4.0 @Frequency 1000 Hz, Temperature 73.4 °F |
DAM; IEC 60250 | |
| Dielectric Strength | 16.5 kV/mm @Temperature 23.0 °C |
419 kV/in @Temperature 73.4 °F |
DAM; IEC 60243-1 |
| Dissipation Factor | 0.015 @Frequency 1000 Hz, Temperature 23.0 °C |
0.015 @Frequency 1000 Hz, Temperature 73.4 °F |
DAM; IEC 60250 |
| 0.018 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
0.018 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; IEC 60250 | |
| Comparative Tracking Index | 575 V @Temperature 23.0 °C |
575 V @Temperature 73.4 °F |
DAM; IEC 60112 |
| 575 V @Temperature 23.0 °C |
575 V @Temperature 73.4 °F |
DAM; UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
| 320 - 330 °C | 608 - 626 °F | DAM | |
| Mold Temperature | 150 °C | 302 °F | DAM; optimum |
| 140 - 160 °C | 284 - 320 °F | DAM | |
| Drying Temperature | 100 °C | 212 °F | DAM |
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
| Moisture Content | <= 0.10 % | <= 0.10 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black Color | DAM |
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Filler | Glass Fiber reinforcement | DAM |
| Forms | Pellets | DAM |
| Generic | Polyphthalamide (PPA) | DAM |
| Heat Stabilized | Yes | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA6T/XT-GF15< | ISO 11469; DAM |
| >PPA-GF15< | SAE J1344; DAM | |
| Polymer Family | High performance polyamide | DAM |
| Polymer Type | Partially Aromatic PA, PPA | DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Glass Reinforced Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA6T/XT-GF15 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Ultrasonic Weldable | Yes | DAM |