Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.50 GPa | 943 ksi | |
Plastcom SLOVAMID 6 GF 20 FRG 3 PA6, 20% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 20 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 9.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 HS-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 SG-GV 1515 Nylon 6.6 for injection molding, 15% mineral filled and 15% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Nilit FRIANYL A63 W-GV25 Nylon 6.6, std. viscosity for injection molding, 25% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.50 GPa @Temperature 23.0 °C |
943 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D638 |
Gharda Chemicals Gafone S 1320GF Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
DSM Akulon® K224-G3U (Dry) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Grupo Repol Dinalon® A1S25 G15 PA66 15% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® SF 2230 Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527-2 |
Styron LGF 9621 Homopolymer Polypropylene Overview: LGF 9621 is polypropylene homopolymer reinforced with 60% by weight of long glass fibers. (PP-LGF60, Long Glass fiber Granulate). This PP-LGF60 is a ‘concentrate’ which has to be.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Polyram RamTough PZ307G6 Polycarbonate, 30% Glass Fiber, UV Stabilized 30% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K222-KGV5 25% Glass Reinforced, Flame Retardant (Halogen free), Heat Stabilized |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BM-30 PA6-MD30 Product description: Grilon BM-30 is a 30% mineral reinforced PA6 injection moulding grade. Grilon BM-30 has the following important properties: heat stabilizedimpact resistantisotropic shrinkagelig.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G15HSL BK363 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G15HSL BK363 is a 15% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 1560 T8 GF ABS / Nylon 6 Blend, 30% Glass & Mineral Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.30% glass fiber and mineral fillerGood impact strength, high chemical resistance, excellent heat resistance, high dimension.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | ASTM D638 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Tensile Modulus | 6.50 GPa | 943 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 35 CX H2.0 900876 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |