Mechanical Properties Metric English Comments
Flexural Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Flexural Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.75%); ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 5.80 GPa

@Temperature -40.0 °C
841 ksi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..